VikingPyrotechnics Posted December 30, 2013 Posted December 30, 2013 Hi guys, here a Beraq shell. in the shell were four rings of salutes. 2 separate, and the last two rings simultaneously. The first two I have "traditional" timed.(Slurry) The timing was not very good. But it was my first attempt and definitely not my last. https://www.youtube.com/watch?v=2Gm4dnwqbRg GreetsVP
BJV Posted December 30, 2013 Posted December 30, 2013 That unsecured mortar is a VARY BAD idea....BJV
VikingPyrotechnics Posted December 30, 2013 Author Posted December 30, 2013 you're right. you can see it bad, but the mortar was a little deeper in the ground. Not much, only so much he could not tip over.
LambentPyro Posted December 30, 2013 Posted December 30, 2013 Great job, not bad! What type of fuse did you use for the salutes?
VikingPyrotechnics Posted December 30, 2013 Author Posted December 30, 2013 Thank you :-)the first two "rings" were traditionally timed with slurry. the last with bickford.
Niladmirari Posted January 16, 2014 Posted January 16, 2014 Good job. What composition for white smoke?
Recommended Posts