Here is my new years show was a big disappointment the e-match and the one of 2 shoots failed completely, the shells that did go off were pretty good. Need to find a new supplier.........bonus have extra shells for the 4th.

 

Posted

"if that had cracklin in it, that'd be a crackling palm!" hahaha.... nice work!

 

What formula where the silver stars, they had a nice hang to them?

Posted (edited)
I had a fusing problem with my shoot too. It ended up being seperated in 3 parts--which was shitty--because of the "master fuse"'s failure to take fire, twice! Edited by AirCowPeacock
Posted

"if that had cracklin in it, that'd be a crackling palm!" hahaha.... nice work!

 

What formula where the silver stars, they had a nice hang to them?

I like this silver tooo those were rolled stars

Potassium Nitrate

50

 

 

 

Titanium, sponge, 40-80 mesh

27

 

 

 

 

Charcoal Airfloat

10

1

 

 

Sulfur

8

 

 

 

Dextrin

5

Posted
no wonder they're bright, look at all that titanium! :D
×
×