californiapyro Posted May 23, 2012 Posted May 23, 2012 This is an idea I had for using the new magnesium chips from Skylighter. they make very bright and long tails. I use mineral oil to bind the mixture, and was wondering if this would hold up to the burst of a shell. any thoughts? http://www.youtube.com/watch?v=sqa6QrJUPEw
warthog Posted May 23, 2012 Posted May 23, 2012 I will call Harry and tell him to give you the prizes. Rock On Cali!
californiapyro Posted May 23, 2012 Author Posted May 23, 2012 haha, thanks warthog fingers crossed no one else enters
Mumbles Posted May 23, 2012 Posted May 23, 2012 If it doesn't hold up to a shell burst on it's own, I'd put my money on lack of compaction. An arbor press final compaction or something should fix that right up. Looks good.