petroleum Posted June 25, 2011 Posted June 25, 2011 (edited) Hi All!Its my 4 incher. Stars C8+8%Ti (flake) to Red (modified comp. by Karlos: KClO4-40;Sr(NO3)2-20; MgAL-17; Parlon -15 (original PVC); charcoal-2; phenolic resin - 6 (original red gum)). Red cores - 4x4x4 mm cubic stars (solvent EtOH). Coated with Hot Prime by Shimizu. C8 comp was ball milled for 3 hours. Solvent EtOH/H2O=50/50. Burst charge - H3 on granulated tea. Lift charge - meal on granujlated tea. http://www.youtube.com/watch?v=pP37V8dA_Zw Edited June 25, 2011 by petroleum