Mraliksr Posted April 3, 2022 Posted April 3, 2022 the comp I'm using is: bismith subcarbonate 75gmagnalium 200 mesh 15gcopper II oxide 10gn.laquer 10% the eggs are maybe 2-4 mm in size. very hard to light even with a primer. real loud pop when they do light.Greeting Sir, I have tried lead trioxide bismuth all kind nothing explode or crackling
SharkWhisperer Posted April 3, 2022 Posted April 3, 2022 Greeting Sir, I have tried lead trioxide bismuth all kind nothing explode or cracklingResponding to a 10 year-old post? 35:35:30 BiO3/CuO/MgAl, primed properly. Works. Check your chems. Check your priming. Check your MgAl:star sizing. Crackle/DEs are really not difficult. Bind with NC or bind with phenolic resin like the Chicoms do. Simples.