White star- Hey guys these star burns pretty white in colour without leaving tail.

 

Sodium Nitrate........6

 

barium nitrate........2

 

sulphur.........2-1/4

 

charcoal(air).....1/2

 

mg(fine)......1

 

mg(coarse).....1

 

 

  • Like 1
Posted
uncoated magnesium and nitrates (especially ones like sodium) are known for their spontaneous ignition I hope your using coated magnesium
Posted

uncoated magnesium and nitrates (especially ones like sodium) are known for their spontaneous ignition I hope your using coated magnesium

 

Obviously I use coated Mg

  • Like 1
Posted
it wasn't obvious and it is your responsibility to alert possible users of your formula to the extreme dangers if they follow it as it is set out
Posted

This composition I used: and it very good for me, easy to roll:

 

White star #1

Potasium nitrate...........................................57

Sulfur.....................................................23

Black powder...............................................20

Dextrin....................................................+4

Posted

it wasn't obvious and it is your responsibility to alert possible users of your formula to the extreme dangers if they follow it as it is set out

note-all part by weight.

Sodium nitrate.....6

Barium Nitrate......2

sulphur.....2-1/4

Charcoal(air).....1/2

Mg(fine,coated)......1

Mg(coarse,coated).....1

  • Like 1
Posted

White metal fuelled compositions are usually designed without sulphur. Sodium nitrate give yellow colour to flame and in the white formula isn´t important. Where is binder?

Insufficient formula.

  • 5 months later...
Posted

This composition I used: and it very good for me, easy to roll:

 

White star #1

Potasium nitrate...........................................57

Sulfur.....................................................23

Black powder...............................................20

Dextrin....................................................+4

 

What can I use as a prime? I tried BP but it didnt work too well.

 

Posted
Try a pinch of silicon metal in the prime, it helps get lower fuel comps going.
Posted (edited)

Try a pinch of silicon metal in the prime, it helps get lower fuel comps going.

 

Hum. Don't have any. Could I add some Ti or Al instead?

Edited by pillyg
Posted
Nope, they will not do the same thing. The silicon turns to tiny molten glass and helps ignite hard to light comps. The metals all burn away.
Posted
Ok
Posted
I just ignited some with my SUPER slow KNO3/Al/S flash. I dont think that would be a good prime though.
Posted
Sure, why not? Use BP over the top of the slo-flash. Make a small mine and see how it does or better yet, shoot some from a star gun.
Posted
Hum. Ok I will try that. I just remember hearing that KNO3/Al was unstable and that water+Al=bad but if you say its ok, I believe you
Posted
Treat the aluminum with boric acid first, that will keep the reaction down.
Posted

What can I use as a prime? I tried BP but it didnt work too well.

I have no problem with these star, prime with BP (milled 15min) catch fire very easily.. By the way, this composition of star I also milled about 30min.. that's why so easy it light ;)

Posted
Ok. I finally got to work but it seemed like I used a lot of prime.
Posted
They are probably not dry yet. KNO3 and dextrin comps can take quite a while to dry out. I am on week three for a batch of stars I made and year two on a batch of TT that I made in 2009. :huh:
Posted
Haha thats a lot. I tried a desecator bag but it didnt really work. I had calcium chloride
×
×