We are looking into the use of copper thermite to create igniters capable of burning at higher temperatures than standard commercial igniters. To initiate the reaction, we are using nichrome wire attached to the ends of our copper wires. However, we are uncertain about the best binder to use with the thermite to effectively mold it around the copper/nichrome wire assembly. Do you have any recommendations for a binder or alternative methods to develop exceptionally high-temperature igniters?

×
×