MADBOY Posted January 13 Posted January 13 In here I am use Red lead 800 Cu 150 Maglelium 180 Automise aluminium powder 25 I am test I am very scared because the sound is very danger and also very loud VN20240113_172456.mp4
Mraliksr Posted October 27 Posted October 27 Greeting Sir with thanks, kindly note my crackling or dragon eggs not getting ignition easily burn and red like iron red in heat not explode binding with nc lacquer lead tetraoxide 75 maganlium 15 copper oxide 10 nc 10 thanks for guide
Zumber Posted October 27 Posted October 27 Is all your chemicals pyro grade specially NC ? What mesh magnelium did you used?