fr3dopyrox Posted February 21, 2021 Posted February 21, 2021 (edited) Hello friends, I have blue chlorate organic and red chlorate stars, i will burst with h3 , i only granulats h3 , and if i can mix simple rice hulls with h3 granulate for slow down the breack and dont shattering my little stars:12 mm , my ball shell is 2,5 inch and 4 inch , and do you think 2 layers of maltese pasting is enough? What do you think ? Thanks you guys Edited February 21, 2021 by fr3dopyrox
pyrojig Posted February 21, 2021 Posted February 21, 2021 You can coat on hulls to slow down and reduce the amount of burst in the shell . The critical part is size control with the mesh with the of the granulated h3. Must be consistent, and carefully sifted to give perfect breaks you can recreate . As you may already know , most chlorate stars don't usually need prime, but it wouldn't hurt to get complete ignition on the whole star surface .Paste layers vary on h3 breaks. Start with a couple less layers than called for in commercial bursts.