Hi Folks,

 

Not having access to fine mesh screens (80 - 100 mesh), also at some point I know coffee grinders can only get materials so fine. The material in question is magnallium. Anyone have an idea what an approx mesh size a well ground mgal would be?

 

DaM

Posted

The reason for the question is that I attempted to make some 60/40 (KCLO4/MgAl), and it would not light with a fuse either in the open or confined. Which lead to think the mesh size.

 

DaM

Posted

well ground mg/al should/would be -325 mesh. It's basically like what you'd expect from German Black Aluminum.

 

Also, try 50/50 Potassium Perchlorate and Magnalium... that should burn like you'd expect.

×
×