Have a look at F.A.S.T. p.217 and use finer mg then specified.
  • 1 year later...
Posted

i primed my fuses with NC lacquer that i mixed some meal powder into and it works every time. I made the NC lacquer from ping pong balls. Does anyone know what is a good container to store NCl lacquer i have mine in a canning jar but the acetone keeps eating away at the gasket on the jar lid then the acetone evaporates out.

I use the same pingpong nclacquer and store it in glass jam pot (3years using the same pot...) no issues..

Posted

I ran through my supply of good ping-pong balls. Tried some from Academy Sports and they weren't NC based. I actually like PPB lacquer because it is stickier than that made from double base smokeless powder. I wish I could find decent balls around here.

I store mine in quart metal cans made for paint and it holds well for a long time.

Posted

Dunlop clubmatch are nc if you can find some of those, they`re "made in china" ;)

×
×